What’s Fused Cast

The term Fused Cast refers to a manufacturing process in which the ceramic bonding is obtained by the solidification of a mixture that has been melted in an electric furnace and cast in a liquid state into molds.


► Fused Cast AZS Blocks Introduction

AZS fused cast block is also called fused cast block which is abbreviated as AZS because it contains Al2O3-ZrO2-SiO2. Fused cast AZS block is made from pure alumina powder and Zircon sand (composed of 65% zirconia and 34% SiO2). After Alumina powder and zircon sand melting in an electric furnace, they are cast into various molds and cool themselves down to become white solid. Because of the different content of Zirconia from 33%-41%, our fused cast AZS blocks can be divided into three types AZS—33#, AZS—36#, and AZS—41#.

►TY-AZS33 Description

Fused cast AZS 33# block has a dense microstructure which ensures its great resistance in glass liquid, thus you don’t have to worry about the solidification and other problems. It is widely applied to glass furnaces for the superstructure, working pool sidewall, paving blocks, feeder channels, tank bottoms, C-shaped block, and doghouse crown, etc.

►Advantages

1. Compact microstructure
2. Good erosion resistibility to molten glass
3. Good thermal shock resistibility, high compression resistance
4. Barely rendering blister
5. A variety of formats and shapes for furnace different working areas

Different casting methods can produce various shapes and sizes of AZS for
different areas of glass furnaces

►Choose Us

TY-AZS series blocks have passed the ISO international certification. High purity raw material, scientific formula, advanced technology, and professional guide all contribute to our qualified as blocks production. Over 30 years of producing and marketing experience, we have developed a stable customer base overseas and kept long-term cooperation. Need refractories for high-temperature furnace fuel? Contact us, We will never let you down.

fused cast azs ty azs336

■ Technical Data

Item TY-AZS33
Chemical Composition Al2O3 ≥50.00
ZrO2 ≥32.50
SiO2 ≤15.50
Na2O+K2O ≤1.30
Bulk density g/cm3 ≥3.85
Apparent Porosity % ≤1.2
Cold Crushing Strength Mpa ≥300
Exudation Temperature of Glass Phase ≥1400
Bubble Separation Ratio(1300℃×10h) ≤1.5
Apparent density (g/cm3) PT(RN RC N) ≥3.45
ZWS(RR EVF EC ENC) ≥3.60
WS( RT VF EPIC FVP DCL) ≥3.70